A sink mark is a shallow depression or dip that forms on the surface of a plastic model part during manufacturing. It is not a hole or a crack, but a slight sunken area that catches light and stands out once you paint the part. The term is informal hobby slang, but every modeler knows exactly what it means.
Spot a Sink Mark Before You Paint
Sink marks usually appear on flat or slightly curved surfaces, often near thick sections of plastic or where a part attaches to the sprue. The plastic shrinks as it cools in the mold, and the thinner outer skin sinks inward. You will see them on fuselage halves, wing roots, and sometimes on the backs of panels or doors.
Look for them in good light, tilting the part so the surface catches a reflection. Run a fingertip across the area; a sink mark feels slightly lower than the surrounding plastic, but it does not catch your nail like a scratch. If you are not sure, wipe the part with a bit of thinner on a cloth and look again under a bright lamp.
Check every part before you assemble, because once the model is together, filling a sink mark means sanding across panel lines and detail. Catching it early saves work.
Fill Sink Marks With the Right Material
You have three common choices for filling a sink mark: putty, CA glue, or a drop of liquid cement mixed with plastic shavings. Each works, and the best choice depends on the size of the dip and what you have on hand.
For a small, shallow mark, a smear of putty is the quickest fix. Apply it with a toothpick or a small spatula, pressing it into the dip, and let it dry fully. Then sand with fine grit sandpaper, starting at a medium grit and working down to a very fine one. Feather the edges so the repair blends into the surrounding plastic.
For a tiny mark, a drop of CA glue can work. Put a small amount in the dip, let it cure, then sand. CA glue dries hard, so be careful not to overfill and sand into the surrounding surface. For larger sink marks, some modelers mix plastic shavings from the sprue with liquid cement to make a thick paste. This bonds well with the part, but it takes practice to get the consistency right.
Whichever filler you choose, test it on a spare sprue first. Some putties shrink as they dry, and some CA glues are harder than the plastic, which makes sanding tricky. The label on the product usually tells you the drying time and how it sands.
Sand and Polish the Repair Smooth
After the filler is dry, sand the area with fine grit sandpaper, using a small block or a sanding stick to keep the surface flat. Start with a medium grit, like 400, then move to 600, then 800, and finish with 1000 or higher if you need a smooth finish. Wet sanding, where you dip the paper in water, reduces dust and helps the paper last longer.
Check your progress often. Sand in one direction, then wipe the surface with a cloth and look at it in the light. The goal is to make the filled area level with the surrounding plastic, not to remove all the paint or primer. If you sand too much, you can create a low spot, which is worse than the original sink mark.
After sanding, run your finger over the spot. It should feel perfectly smooth, with no edge where the filler meets the plastic. If you still see a faint line, apply a thin coat of primer and look again. Primer often reveals small imperfections that are invisible on bare plastic.
Prime and Paint to Hide the Repair
Once the surface is smooth, apply a coat of primer. Primer fills tiny scratches and gives the paint a uniform surface to grip. Let the primer dry, then inspect the area again. If the sink mark is still visible, you may need to repeat the filling and sanding process. If it looks good, you can proceed with your normal painting.
Paint color and finish matter. A glossy, light color will show any remaining imperfection, while a matte, dark color hides more. If you are painting a light color, take extra care with the sanding. If you are painting a dark color, you might get away with a less perfect repair.
Remember that paints and thinners interact differently with different fillers. Test your paint on a spare piece of the same filler to make sure it does not react or cause the filler to soften. Follow the paint label’s instructions for thinning and application.
Prevent Sink Marks on the Next Kit
You cannot prevent sink marks that come from the mold, but you can avoid making them worse. Do not use too much glue when joining parts; excess glue can soften the plastic and create a depression. Also, be careful when removing parts from the sprue. If you cut too close to the part, you can leave a stress mark that looks like a sink mark.
Some modelers use a technique called “rescribing” after filling a sink mark. If the sink mark is on a panel line, you may need to re-cut the line with a scribing tool after sanding. This is a separate skill, but it is worth learning if you build models with lots of panel detail.
Finally, think about the order of your build. Fill and sand all sink marks before you assemble the major parts. Once the fuselage is glued together, accessing a sink mark inside a wheel well or under a wing is much harder. A little planning saves you from awkward sanding later.
Know When a Sink Mark Is Not a Sink Mark
Sometimes a depression is not a sink mark. It could be a short shot, where the plastic did not fully fill the mold, leaving a gap or a thin spot. It could also be a knock-out pin mark, which is a small round depression left by the ejector pins in the mold. These look similar but are usually smaller and rounder.
If the depression is deep and has a sharp edge, it might be a defect in the plastic, like a void or a bubble. In that case, the part may be weak, and you might want to reinforce it or replace it if you have a spare. Sink marks are shallow and smooth, so if you feel a sharp edge, treat it differently.
When in doubt, check the kit instructions to see if the part is visible on the finished model. If it is hidden, you can ignore the sink mark. If it is on an exterior surface, take the time to fix it. A few minutes of filling and sanding makes a big difference in the final look.
Safety
Safety: dust from sanding, drilling or cutting resin parts, putty and fillers is harmful to breathe and can irritate skin and eyes. Sand wet where you can, wear a respirator rated for fine particulates and eye protection, work with good ventilation, and wipe dust up with a damp cloth instead of blowing it away. Liquid and uncured resins can irritate or sensitise skin, so wear nitrile gloves when handling them. Read the label and the safety data sheet that come with the product.
Safety: many model paints, thinners, cements, lacquers and putties give off solvent vapour that is harmful to breathe, and many are flammable. Work with good ventilation, keep them away from flames and heat, keep lids closed, and follow the label and the maker’s safety data sheet. When airbrushing, use a spray booth that vents outdoors and wear a respirator suited to the paint you are spraying (the label or safety data sheet says which); a dust mask alone does not stop solvent vapour.
Safety: cyanoacrylate (super) glue bonds skin and eyes in seconds and its fumes can irritate eyes and airways, and plastic cements contain solvents. Use them with ventilation, keep the nozzle pointed away from your face, keep a debonder nearby, and follow the label. Get medical help if glue gets into an eye.