Yes, you can fix air bubbles in resin model parts, and the method depends on whether the bubble is on the surface or trapped inside. Surface bubbles are the most common and the easiest to repair, while internal bubbles need a different approach. Here is the direct fix for each case, then the steps to make the repair invisible.
Surface Bubbles: Fill and Sand
Surface bubbles are small craters or pinholes that open to the outside of the part. They show up after you prime or paint, because the paint sinks into the hole. To fix them, you need to fill the hole with a material that dries hard and sands smooth.
Your options are:
- Thin CA glue (super glue) – it wicks into the hole and dries hard.
- Two-part epoxy putty – good for larger craters.
- Mr. Surfacer or a similar liquid putty – designed for this job.
Whichever you choose, apply a small amount with a toothpick or a fine brush. Overfill slightly, because the filler will shrink as it dries. Let it cure completely – the label will tell you how long. Then sand the area flat with fine sandpaper, starting around 400 grit and working up to 1200 or finer. Re-prime and check. If the bubble is still visible, repeat the fill and sand once more. This usually does the trick.
Internal Bubbles: The Drill-and-Pin Method
Internal bubbles are air pockets completely enclosed inside the resin. You can’t see them until you cut or sand into the part, and then you find a void. The fix is to open the bubble to the surface, fill it, and then sand.
Here is the step-by-step:
- Find the bubble by tapping the part – a hollow sound can indicate a void. Or you may see a faint dark spot under the surface.
- Drill a small hole into the bubble with a pin vise or a hand drill. The hole gives the filler a way in and lets trapped air escape.
- Fill the hole with CA glue or epoxy putty, pressing it in well. Overfill slightly.
- Let it cure, then sand smooth. If the bubble is deep, you may need to fill in layers, letting each layer dry before adding the next.
For a large internal void, you can also cut out the bubble with a rotary tool, creating a clean cavity, then fill it with epoxy putty. This works well but takes more patience.
Why Bubbles Form in Resin Castings
Bubbles happen during the casting process. When liquid resin is poured into a mold, air can get trapped in corners, undercuts, or thin details. If the resin is not degassed or the mold is not vibrated, those air pockets stay. The result is a part with surface pinholes or internal voids.
Knowing this helps you prevent future problems. When you buy a resin kit, inspect the parts before you start. Look for shiny spots that might be thin resin over a bubble. Tap parts gently – a dull thud can mean a void. If you find a bad bubble before you assemble, you can fix it before painting, which saves you from sanding through paint later.
Where People Go Wrong: Sanding Too Early or Too Late
The most common mistake is sanding before the filler is fully cured. CA glue can feel hard on the outside but still be soft underneath. If you sand too soon, the filler pulls out of the hole, and you are back to square one. Always wait the full cure time listed on the product label.
The second mistake is using too much filler. A big blob of putty creates a lump that is hard to sand flat without damaging the surrounding resin. Use a tiny amount and add more if needed. You can always add, but you cannot easily remove.
A third mistake is ignoring the bubble until after you paint. Paint does not fill bubbles; it highlights them. Prime first, then check for pinholes. Fix them before the final color coat.
Testing Your Repair on a Spare Part
Before you fill a visible bubble on a model part, test your filler on a scrap piece of resin or an old sprue. Apply the same filler, let it dry, and sand it. This tells you how the filler behaves – whether it sands easily, whether it shrinks, and how it takes paint. Paints and fillers interact differently with different resin blends, so a test is always a good idea. Follow the instructions on the filler and the paint labels, and if you are unsure, check the manufacturer’s website.
Once your repair is sanded and primed, you should not see the bubble at all. If you do, it usually means the filler was not fully cured or you did not sand enough. Go back and repeat the fill and sand cycle. With a little patience, the repair will be invisible under paint.
Safety
Safety: dust from sanding, drilling or cutting resin parts, putty and fillers is harmful to breathe and can irritate skin and eyes. Sand wet where you can, wear a respirator rated for fine particulates and eye protection, work with good ventilation, and wipe dust up with a damp cloth instead of blowing it away. Liquid and uncured resins can irritate or sensitise skin, so wear nitrile gloves when handling them. Read the label and the safety data sheet that come with the product.
Safety: many model paints, thinners, cements, lacquers and putties give off solvent vapour that is harmful to breathe, and many are flammable. Work with good ventilation, keep them away from flames and heat, keep lids closed, and follow the label and the maker’s safety data sheet. When airbrushing, use a spray booth that vents outdoors and wear a respirator suited to the paint you are spraying (the label or safety data sheet says which); a dust mask alone does not stop solvent vapour.
Safety: cyanoacrylate (super) glue bonds skin and eyes in seconds and its fumes can irritate eyes and airways, and plastic cements contain solvents. Use them with ventilation, keep the nozzle pointed away from your face, keep a debonder nearby, and follow the label. Get medical help if glue gets into an eye.
Safety: hobby knives, razor saws, sprue cutters and photo-etched parts are very sharp. Cut on a cutting mat, away from your body, with your fingers behind the blade; replace dull blades, because a dull blade slips; cap or store blades safely, and wear eye protection when parts can fly off or when using a rotary tool, whose cutting discs can shatter. Supervise children closely.