The most common wing spar repair is a clean break at the root or mid-span on a built-up or solid balsa wing. You fix it by splicing a new spar alongside the broken one, or by replacing the broken section entirely. The method differs if the spar is carbon fiber or a metal tube, where you need a different joint and adhesive.
Assessing the Break and Choosing a Repair Method
Look at the break first. A clean snap in a wooden spar can be glued and reinforced with a doubler. A crush or splintered break needs the damaged section cut out and replaced. If the spar is hollow or a tube, you may need an internal sleeve rather than an external splice.
Check the surrounding structure. Ribs, sheeting, and the leading or trailing edge may also be damaged. Repair the spar first, then fix the rest. If the wing is covered, you will need to remove the covering over the damaged area to work on the spar.
Wooden Spars: Splice or Replace
For a clean break, cut the two ends square and glue a new piece of the same wood alongside the break, spanning past both sides. This is a splice plate. For a crushed section, cut out the damaged part and glue in a new piece of spar, then reinforce the joints with small plates on both sides.
Carbon Fiber and Metal Spars
Carbon spars often crack or delaminate. Sand the area lightly, then wrap with carbon tow or fiberglass cloth and epoxy. Metal tubes can be repaired with an internal sleeve that fits snugly inside, glued with epoxy. Do not use CA on carbon or metal; use a proper epoxy.
Steps to Splice a Broken Wooden Spar
- Remove the covering from the damaged area, cutting back to the nearest rib on each side.
- Cut the broken spar ends square with a sharp knife or razor saw. Remove any crushed or splintered wood.
- Cut a splice plate from the same type of wood, long enough to extend at least twice the spar depth past each side of the break.
- Glue the splice plate to one side of the spar with wood glue or epoxy. Clamp it until the glue sets, following the glue label for curing time.
- Add a second splice plate on the opposite side for a stronger joint. This sandwiches the spar.
- If the break is at a rib, glue the splice to the rib as well to spread the load.
- Sand the repair smooth and blend it with the surrounding wood.
- Re-cover the area with matching covering material, using the same iron or heat settings as the original.
What the Repair Depends On
The size of the splice plate and the type of glue depend on the spar’s dimensions and the model’s weight. Check the kit instructions or the wood’s grain direction. For a typical balsa spar, a splice plate about the same thickness and twice the length of the spar’s depth works. For heavier models or larger spars, use a longer plate and epoxy instead of CA.
Glue Choice
Wood glue (aliphatic resin) is strong and dries clear, but needs clamping. CA (cyanoacrylate) is fast but brittle. Epoxy is strongest for structural repairs, but takes longer to cure. Test the glue on scrap wood first to see how it flows and sets.
Mistakes That Cause a Weak Repair
One common mistake is gluing the break without a splice plate. A butt joint is weak and will fail again. Another is using too small a splice plate, which does not spread the load enough. A third is not removing all the crushed wood, leaving a weak point. Finally, using the wrong glue, like CA on a joint that flexes, can crack under load.
How to Tell It Worked
After the glue cures, flex the wing gently. It should feel as stiff as the undamaged side. Check that the splice plates are fully bonded with no gaps. If you can see a gap, add more glue and clamp again. The wing should hold its shape and not twist.
Repairing a Carbon Fiber or Metal Spar
For carbon, sand the damaged area to roughen it, then wrap with carbon fiber cloth and epoxy. Let it cure fully. For metal tubes, cut a sleeve that fits inside the tube, coat it with epoxy, and slide it into one side, then the other. Clamp the joint until set. Always follow the epoxy label for mixing and curing times.
When the Spar Is Beyond Repair
If the spar is shattered into many pieces or the wing is badly twisted, replacement may be easier. Cut the old spar out and make a new one from the same wood. Use the old spar as a template for length and shape. Glue the new spar into the wing, aligning it with the ribs and the wing’s dihedral.
Checking Dihedral and Alignment
Before gluing, lay the wing on a flat board and check that the dihedral angle matches the other wing. Use a protractor or a template from the kit. If the spar is off, the wing will twist. Adjust the fit before gluing.
After any repair, check the wing for warps. A twisted wing will affect how the model flies. If you are not sure, ask a more experienced builder or check the kit instructions.
Safety
Safety: dust from sanding, drilling or cutting resin parts, putty and fillers is harmful to breathe and can irritate skin and eyes. Sand wet where you can, wear a respirator rated for fine particulates and eye protection, work with good ventilation, and wipe dust up with a damp cloth instead of blowing it away. Liquid and uncured resins can irritate or sensitise skin, so wear nitrile gloves when handling them. Read the label and the safety data sheet that come with the product.
Safety: cyanoacrylate (super) glue bonds skin and eyes in seconds and its fumes can irritate eyes and airways, and plastic cements contain solvents. Use them with ventilation, keep the nozzle pointed away from your face, keep a debonder nearby, and follow the label. Get medical help if glue gets into an eye.
Safety: hobby knives, razor saws, sprue cutters and photo-etched parts are very sharp. Cut on a cutting mat, away from your body, with your fingers behind the blade; replace dull blades, because a dull blade slips; cap or store blades safely, and wear eye protection when parts can fly off or when using a rotary tool, whose cutting discs can shatter. Supervise children closely.