Most gaps on model float struts come from the joint where the strut meets the float or the fuselage. The usual fix is to fill the seam with a gap-filling super glue or a model putty, then sand it flush. If the strut is a separate piece that flexes, the method changes: you need a filler that stays slightly flexible, or you reinforce the joint before filling.
Pick the Filler for the Strut Material
What you use depends on what the strut is made of. Injection-molded polystyrene struts take standard model putty or gap-filling cyanoacrylate (CA) glue. Resin struts need a putty made for resin, or CA works too. Wooden struts (common on older kits or scratch builds) take wood filler or CA. If the strut is part of a vacuform or a soft plastic, test the filler on a spare sprue or hidden area first, because some putties attack soft plastics.
For a gap that is thin and shallow, CA glue alone works. For a wider or deeper gap, use a two-part epoxy putty or a solvent-based model putty. Always check the label on the putty or glue to see which plastics it is safe for, and test on a scrap piece if you are unsure.
Prepare the Joint Before You Fill
Clean the parts with warm soapy water or a mild solvent to remove mold release and grease. Dry them fully. Dry-fit the strut to the float or fuselage and see where the gap is widest. If the strut rocks or sits crooked, sand the mounting face flat before filling, otherwise the filler will crack later. Use a small file or sandpaper on a flat surface to true the end of the strut.
Mask off the areas around the gap with low-tack tape. This keeps filler off the surrounding surface and makes sanding easier. If the gap is at the float, tape the float’s hull so you do not scratch it.
Fill the Gap in Layers
- Apply the filler with a toothpick or a small spatula. Press it into the gap, slightly overfilling so it stands a little proud of the surface.
- For a deep gap, fill in layers. Let the first layer cure, then add a second. Do not try to fill a deep hole in one go, because the filler can shrink as it cures.
- If you are using CA glue, use a thin or medium viscosity and apply it with a fine applicator tip. You can also use a CA glue with a built-in brush. For a large gap, sprinkle a little baking soda over the wet CA to build it up, then add more CA. This creates a hard, sandable filler. (Note: baking soda accelerates CA and generates heat, so use it in thin layers and let it cool.)
- For two-part epoxy putty, knead the two parts together until the color is uniform, then press it into the gap. Smooth the surface with a wet finger or a tool dipped in water.
- Let the filler cure fully. Curing time depends on the product; check the label. Do not rush sanding while it is still soft.
Sand and Shape the Filled Area
Once cured, sand the filler flush with the surrounding surface. Start with a medium grit sandpaper (around 240 to 320) and work down to a fine grit (400 to 600). Use a sanding block for flat areas, and a small file or folded sandpaper for curves. Keep the sandpaper wet if you are using water-resistant paper; this keeps dust down and gives a smoother finish.
Check the joint by running a fingernail across it. If you feel a ridge, sand a little more. If you sand through the filler and expose the gap again, apply another thin layer and repeat.
After sanding, wipe off the dust with a tack cloth or a damp cloth. The surface is now ready for primer. Prime the filled area to see if any pinholes or low spots remain. If you see them, fill those spots with a thin layer of putty or CA, sand again, and re-prime.
When the Strut Flexes: Use a Flexible Filler
If the strut is a separate piece that will flex during handling or flight (on a radio-control model, for example), a rigid filler will crack at the joint. Use a flexible filler, such as a flexible CA glue or a rubberized model filler. These are sold as “flexible” or “rubber-toughened” CA. Apply it the same way, but do not overfill; a thin layer is enough to fill the gap. Sand it gently with fine grit, because flexible fillers do not sand as easily as rigid putty.
For a stronger fix on a flexing joint, reinforce the inside of the strut before filling. Glue a small strip of plastic card or a wire inside the strut, spanning the joint, then fill the outside. This spreads the load and prevents the filler from cracking.
What Goes Wrong and How to Fix It
- Filler shrinks and leaves a low spot. This happens when you apply too thick a layer. Sand the low spot, apply a thin skim coat, and sand again.
- Filler cracks after drying. The joint is flexing, or the filler is too rigid for the plastic. Use a flexible filler or reinforce the joint from behind.
- Filler melts the plastic. You used a solvent-based putty on a soft plastic. Stop, sand off the damaged area, and switch to a water-based or CA filler. Test on a spare part first.
- Filler is hard to sand. It may not be fully cured, or you are using too coarse a grit. Wait longer, or use a finer grit with a sanding block.
Before You Start: A Quick Checklist
- Clean parts with soapy water or mild solvent and dry them.
- Dry-fit the strut and check the gap size.
- Choose a filler that matches the strut material (polystyrene, resin, wood, or soft plastic).
- Test the filler on a spare sprue or hidden area if you are unsure.
- Mask off the surrounding surface with low-tack tape.
- Have sandpaper in medium and fine grits, a sanding block, and a tack cloth ready.
If you are working with paints, glues, or putties, see the safety notes below for ventilation and skin protection. Always follow the label instructions on any product you use.
Safety
Safety: dust from sanding, drilling or cutting resin parts, putty and fillers is harmful to breathe and can irritate skin and eyes. Sand wet where you can, wear a respirator rated for fine particulates and eye protection, work with good ventilation, and wipe dust up with a damp cloth instead of blowing it away. Liquid and uncured resins can irritate or sensitise skin, so wear nitrile gloves when handling them. Read the label and the safety data sheet that come with the product.
Safety: many model paints, thinners, cements, lacquers and putties give off solvent vapour that is harmful to breathe, and many are flammable. Work with good ventilation, keep them away from flames and heat, keep lids closed, and follow the label and the maker’s safety data sheet. When airbrushing, use a spray booth that vents outdoors and wear a respirator suited to the paint you are spraying (the label or safety data sheet says which); a dust mask alone does not stop solvent vapour.
Safety: cyanoacrylate (super) glue bonds skin and eyes in seconds and its fumes can irritate eyes and airways, and plastic cements contain solvents. Use them with ventilation, keep the nozzle pointed away from your face, keep a debonder nearby, and follow the label. Get medical help if glue gets into an eye.
Safety: fine dust from sanding, scraping or grinding pastels, pigments, fillers and plastics should not be breathed. Work on a tray, avoid blowing dust around, wear a dust mask or respirator rated for fine particulates, and clean up with a damp cloth. Check the label of pigments and powders for any extra warnings. Some white-metal castings contain lead: wash your hands after filing or sanding them, and do not eat or drink while you work.