Success looks like a perfectly flat surface with no visible seam or depression, ready for primer. The whole process takes a few minutes per spot, plus drying time for the filler. Start by letting the filler cure completely, then work through progressively finer grits.
What Grit Sandpaper Do You Need?
You will need three grits: coarse, medium, and fine. Coarse grit, around 80 to 120, shapes the filler down to the surrounding level. Medium grit, around 180 to 240, removes the scratches left by the coarse paper. Fine grit, around 320 to 400, gives a smooth surface that primer will grip well.
For sink marks in plastic or wood, start with coarse only if the filler is proud of the surface. If the filler is already level, skip straight to medium. The exact grits on your sandpaper label may vary; the idea is to move from rough to smooth in two or three steps.
How to Sand Sink Marks Smooth After Filling
- Wait for the filler to dry completely. Check the label for the recommended drying time; it often depends on the filler thickness and room humidity.
- Sand with coarse grit using a sanding block or your fingers. Use light, even pressure and keep the paper flat against the surface. Sand in small circles or back-and-forth strokes, checking often to avoid sanding through the surrounding paint or clear coat.
- Wipe away the dust with a tack cloth or a soft, dry cloth. Look at the surface under a bright light at an angle; you want to see the filler level with the surrounding area, not a dip or a bump.
- Switch to medium grit and sand the same area again. This removes the deep scratches from the coarse paper. Keep the paper flat and use a light touch.
- Wipe the dust again and check for any remaining sink marks. If you still see a slight depression, apply another thin coat of filler and repeat from step one. If it looks level, move on.
- Finish with fine grit to polish the surface. This step makes the filler blend invisibly with the surrounding material. Sand lightly and evenly until the surface feels smooth to your fingertips.
- Wipe the area one last time with a tack cloth. The surface is now ready for primer, paint, or clear coat, depending on your project.
How to Tell It Worked
Run your fingertip across the filled spot. It should feel perfectly smooth, with no edge or dip. Look at the surface under a raking light, meaning a light source held low and at an angle; any low spot will show as a shadow. If you see a shadow, the sink mark is still there. You can also use a straightedge, like a ruler, held across the area; any gap under the straightedge means the surface is not flat.
The One Failure Everyone Hits and Its Fix
The most common mistake is sanding too soon. Filler that looks dry on the surface can still be soft underneath. When you sand it, the soft filler smears or tears, leaving a rough, uneven patch. The fix is simple: wait longer than you think you need. Read the filler label for the full cure time, not just the touch-dry time. If the filler is already smeared, let it harden fully, then sand again with coarse grit to level it out.
How Long Should You Wait Before Sanding?
Drying time depends on the filler type, the thickness of the coat, and the room temperature. Most fillers list a touch-dry time and a full-cure time. Touch-dry means you can lightly touch it without leaving a fingerprint. Full-cure means it is hard enough to sand without clogging the paper. Always go by the full-cure time on the label. In cooler or more humid conditions, add extra time. When in doubt, wait overnight.
Can You Sand Sink Marks Without Filling?
Sometimes a sink mark is so shallow that you can sand it out without filler at all. If the depression is less than the thickness of the surrounding paint or clear coat, you can carefully sand the whole area flat with fine grit. This works on clear coats and some paints, but you risk sanding through to the primer or bare material. Try this only on shallow marks, and check often. If you see a color change, stop and apply filler instead.
What About Sanding Between Coats of Filler?
If a sink mark needs more than one coat of filler, sand lightly between coats. After the first coat cures, sand with medium grit to smooth it, wipe off the dust, then apply a thin second coat. This helps the second coat bond and reduces the amount of sanding you need at the end. Let each coat cure fully before sanding or adding the next.
How to Prevent Sink Marks in the First Place
Sink marks happen when the material underneath shrinks as it dries or cures. To minimize them, apply filler in thin layers rather than one thick glob. Thick filler shrinks more and is more likely to crack. Also, make sure the surface is clean and free of grease before filling; a clean surface helps the filler bond and reduces the chance of the filler pulling away. For large dents, consider using a backing material, like a piece of plastic or metal, to support the filler and reduce shrinkage.
What Sandpaper Grit Do You Use After Filler?
After the filler is level and smooth, you need to prepare the surface for paint. The grit you use after filler depends on what you are painting. For primer, 320 to 400 grit is usually fine. For a topcoat without primer, go to 400 or 600 grit. For a final clear coat, you might go up to 800 or higher. The idea is to leave a surface that the next layer can grip without showing sanding scratches. If you are unsure, test on a spare piece of the same material.
How to Sand Around Curved or Complex Shapes
On flat surfaces, a sanding block keeps the paper flat and prevents dips. On curved or complex shapes, use your fingers or a soft backing pad so the paper conforms to the shape. For tight corners, wrap the sandpaper around a small stick or a pencil eraser. Always sand in the direction of the curve or contour, not across it, to avoid creating flat spots. Check your progress often, especially on edges, where it is easy to sand through the filler or the surrounding material.
What If the Filler Keeps Cracking or Chipping?
If the filler cracks or chips after sanding, the cause is usually a poor bond or too-thick a coat. Make sure the surface is clean and slightly rough before applying filler; a light sanding with coarse grit gives the filler something to grip. Also, apply thin coats and let each cure fully. If the filler is meant for a specific material, like wood or plastic, use the right kind for your project. Check the label to see what materials it is designed for. If the problem continues, try a different type of filler or consult the manufacturer’s guidance.
See the safety notes below for handling fillers and sandpaper dust.
Safety
Safety: dust from sanding, drilling or cutting resin parts, putty and fillers is harmful to breathe and can irritate skin and eyes. Sand wet where you can, wear a respirator rated for fine particulates and eye protection, work with good ventilation, and wipe dust up with a damp cloth instead of blowing it away. Liquid and uncured resins can irritate or sensitise skin, so wear nitrile gloves when handling them. Read the label and the safety data sheet that come with the product.
Safety: many model paints, thinners, cements, lacquers and putties give off solvent vapour that is harmful to breathe, and many are flammable. Work with good ventilation, keep them away from flames and heat, keep lids closed, and follow the label and the maker’s safety data sheet. When airbrushing, use a spray booth that vents outdoors and wear a respirator suited to the paint you are spraying (the label or safety data sheet says which); a dust mask alone does not stop solvent vapour.
Safety: fine dust from sanding, scraping or grinding pastels, pigments, fillers and plastics should not be breathed. Work on a tray, avoid blowing dust around, wear a dust mask or respirator rated for fine particulates, and clean up with a damp cloth. Check the label of pigments and powders for any extra warnings. Some white-metal castings contain lead: wash your hands after filing or sanding them, and do not eat or drink while you work.